This graph shows the weight loss of portland cement and activated fly ash cement concretes exposed to different acids, tested per ASTM C267, Standard Test Methods for Chemical Resistance of Mortars, Grouts, and Monolithic Surfacings and Polymer Concretes. Image courtesy American Concrete Institute’s (ACI’s) May 2013 Concrete International